Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Multibase Multi-Pro® 1012 C Polypropylene Calcium Carbonate Filler, 12% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | Tangent; ASTM D790 |
RheTech Products FRP102-00 Polypropylene, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Oxford Polymers 604-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips EC6755 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Containers and lidsPackaging for foods such as yot, sour cream, delicatessen salads and gravyCold temperature packagingPortion dairy containersFe.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 2 mm/min; ASTM D 790 |
Polimeri Europa Sinkral® D 232/M3 ABS Resin
(discontinued **) Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr.. |
|||
Flexural Modulus | 1.55 GPa @Temperature 60.0 °C |
225 ksi @Temperature 140 °F |
ASTM D790 |
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic
(Unverified D Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ISO 178 |
Total Lacqtene® 2007 TN 61 HDPE pipe
(discontinued **) LACQTENE® 2007 TN 61 is a high density homopolymer polyethylene produced by the gas phase polymerization process.LACQTENE® 2007 TN 61 is best processed between 190 and 230°C.Information provided .. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
M. Holland Company PP200 Polypropylene Homopolymer High ESCRGood heat aging resistanceHomopolymerGood stiffnessApplications: AutomotiveHospital goodsHousehold goodsTable products |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 2-2120 17TOP BU UV-Stabilized 17% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-2120 17TOP BU is a black colored, 17% talc-filled, UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-2120 17TOP BU is developed for producing injection .. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.All info.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
LyondellBasell Petrothene® LM600700 High Density Polyethylene (Blow Molding Grade) ApplicationsPETROTHENE LM 6007-00 resin exhibits very low taste and odor characteristics as well as good rigidity. Typical applications include water, and milk and juice bottles.Regulatory StatusLM.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 1124NA Polypropylene Homopolymer CHARACTERISTICS: GOOD EXTRUDABILITY, LOW GEL CONTAIN LOW SLIP AND ANTIBLOCK ADDITIVES APPLICATIONS: CAST FILM AND TUBULAR BLOW FILM WATER QUENCH CPP FILM FOR FOOD PACKAGING, CPP FILM FOR LAMINATION |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 1125NA Polypropylene Homopolymer CHARACTERISTICS: GOOD EXTRUDABILITY, LOW GEL CONTAIN MEDIUM SLIP AND ANTIBLOCK ADDITIVESAPPLICATIONS: CAST FILM AND TUBULAR BLOW FILM WATER QUENCH CPP FILM FOR FOOD PACKAGING, CPP FILM FOR LAMINATIO.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp FFL21 PE (Asia Pacific) LNP* Lubricomp* FFL21 is a compound based on Polyethylene resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP PPE+PP blend. High Impact, Good Heat Resistance |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1mm/min; ISO 527-2 |
Borealis HE125MO Polypropylene HE125MO is a polypropylene homopolymer intended for injection molding. This grade is characterized by good flow properties and high stiffness in and is specially suitable for high-speed injection mo.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Total PPH 3862 Homopolymer Polypropylene, Fiber Grade Total Petrochemicals Polypropylene 3862 is recommended for high speed melt spinning processes and multifilament yarns like bulk continuous filament (BCF) and continuous filament (CF) fibers. 3862 i.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | At 5 mm/min; ISO 178 |
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 h.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ISO 178 |
Unipetrol PP MONSTEN® GB 005 Polypropylene Homopolymer Applications include injection molding, tapes, and thermoforming. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | Tangent, 16:1 span:depth,0.5in/min; ASTM D790 |
Chevron Phillips Marlex® K608 HDPE Extrusion Molding Resin Resin Type: Ethylene HomopolymerCharacteristics: Good ESCRExceptional RigidityExcellent melt strengthGood whiteness in unpigmented partsApplications: Table topsNursery containersDunnage traysLarge t.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
CPC - Vycom PLAYBOARD™ HDPE Sheet for Modular Playground Systems Playboard Modular Playground Systems consists of 2-color PolyCarve™ co-extruded sheet and Grip X™ slip resistant sheet materials.FEATURES AND BENEFITS Weather resistant- Playboard is UV stabilized.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1.3 mm/min, 1% Secant; ASTM D790 |
Amco PRIMATOP PP HOMO 120 Injection Molding Polypropylene Features:medium viscosityexcellent processabilitygood stiffnessenvironmental stress crack resistanceheat performanceminimal odor and tasteApplications:closuressmall applianceshousewarestoyscontains .. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | Tangent; ASTM D790 |
RheTech Products CC20P200-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790A |
Ineos H35Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | tangent; ASTM D790 |
Spartech PP7240 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790A |
BP Amoco Amoco® Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection molding; Rotary CompressionFeatures: Nucleated, Antistatic, LubricatedTypical applications: Closures, CapsComplies with FDA specification, Title 21, CFR 177... |