Polyplastic Armlen® PP MF 30-3IM Polypropylene, 30% Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced, Impact Modified
Manufacturer Polyplastic Group
Trade Name Armlen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastic Armlen® PP MF 30-3IM Polypropylene, 30% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV resistant, impact modified, heat stabilizedInformation provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0070 - 0.040 cm/cm
0.0070 - 0.040 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
ISO 294-4
Melt Flow 11 - 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 - 13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.0 MPa
2610 psi
ISO 527
Elongation at Break 15 %
15 %
ISO 527
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Processing Properties Metric English Comments
Melt Temperature 230 - 240 °C
446 - 464 °F
Mold Temperature 60.0 °C
140 °F