Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyplastics Duracon® SF-10 Acetal Co-polymer (POM), High impact, Flexible

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Impact Modified
Manufacturer Polyplastics Co.
Trade Name Duracon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastics Duracon® SF-10 Acetal Co-polymer (POM), High impact, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O) and carbon-carbon (-C-C- bond) comonomer groups are incorporated into its main chain. Therefore the copolymer has superior chemical and thermal stability, compared with acetal homopolymer.Acetal co-polymer is well-balanced in terms of mechanical, chemical and thermal properties, and its superior moldability allows it to be widely employed in various industrial fields.Information provided by PolyPlastics.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 45.0 MPa
6530 psi
ISO 527-1, 2
Elongation at Break 60 %
60 %
ISO 527-1, 2
Tensile Modulus 1.90 GPa
276 ksi
ISO 527-1, 2
Flexural Strength 61.0 MPa
8850 psi
ISO 178
Flexural Modulus 1.80 GPa
261 ksi
ISO 178
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
ISO 75-1, 2
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: