Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
Manufacturer Polyplastics Co.
Trade Name FR-PET®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastics FR-PET® BN3030SD Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyPlastics.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 126 MPa
18300 psi
ISO 527-1, 2
Elongation at Break 1.7 %
1.7 %
ISO 527-1, 2
Flexural Strength 215 MPa
31200 psi
ISO 178
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178
Charpy Impact, Notched 0.730 J/cm²
3.47 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 228 °C
442 °F
ISO 75-1, 2
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+16 ohm-cm
7.00e+16 ohm-cm
IEC 60093
Surface Resistance 7.00e+16 ohm
7.00e+16 ohm
IEC 60093
Dielectric Strength 18.0 kV/mm
457 kV/in
IEC 60243-1
Comparative Tracking Index 200 V
200 V
IEC 60112