Polyram PB302G50 Nylon 6, 50% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PB302G50 Nylon 6, 50% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
50% glass fiber reinforced, UV and heat stabilized polyamide approved and listed by W.R.C potable water and NSF/ANSI61 internationalInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
DIN 53479
Water Absorption 4.8 %
4.8 %
DIN 53495
Moisture Absorption at Equilibrium 1.5 %
1.5 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 124
124
ASTM-D785
Tensile Strength, Yield 150 MPa
21800 psi
ASTM-D638
Elongation at Break 3.0 %
3.0 %
ASTM-D638
Flexural Strength 320 MPa
46400 psi
ASTM D790
Flexural Modulus 14.0 GPa
2030 ksi
ASTM-D790
Izod Impact, Notched 1.70 J/cm

@Temperature 23.0 °C
3.18 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
Maximum Service Temperature, Air 110 °C
230 °F
Continuous Use
200 °C
392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
DIN 53482
Dielectric Constant 3.8

@Frequency 1e+6 Hz
3.8

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 80.0 kV/mm
2030 kV/in
VDE 0303/4