Polyram RamOfin PPC104 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamOfin PPC104 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ISO 1183
Linear Mold Shrinkage 0.014 - 0.016 cm/cm
0.014 - 0.016 in/in
ISO 2577
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527
Elongation at Break 115 %
115 %
ISO 527
Flexural Strength 35.0 MPa
5080 psi
ISO 178
Flexural Modulus 1.20 GPa
174 ksi
ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C
187 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C
127 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in