Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamOfin PPC717 Polypropylene, UV Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamOfin PPC717 Polypropylene, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV stabilized polypropylene copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
DIN 53479
Water Absorption >= 0.030 %
>= 0.030 %
DIN 53495
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 78
78
ASTM-D785
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM-D638
Elongation at Break 300 %
300 %
ASTM-D638
Flexural Modulus 1.10 GPa
160 ksi
ASTM-D790
Izod Impact, Notched 6.00 J/cm

@Temperature 23.0 °C
11.2 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
DIN 53461
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
DIN 53482
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
DIN 53482
Dielectric Constant 2.3

@Frequency 1e+6 Hz
2.3

@Frequency 1e+6 Hz
VDE 0303/4