Material Notes:
General purpose ABS for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ISO 2577
Melt Flow 20 g/10 min

@Load 10.0 kg,
Temperature 220 °C
20 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527
Elongation at Break 7.0 %
7.0 %
ISO 527
Tensile Modulus 1.80 GPa
261 ksi
ISO 527
Flexural Strength 76.0 MPa
11000 psi
ISO 178
Flexural Modulus 2.10 GPa
305 ksi
ISO 178
Izod Impact, Notched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB