Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamShine PV300G6 ABS, 30% Glass Fiber

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamShine PV300G6 ABS, 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% glass fiber reinforced, heat resistance and minimal mold shrinkage ABS for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
DIN 53479
Water Absorption 0.12 %
0.12 %
DIN 53495
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
Melt Flow 8.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
8.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM-D785
Tensile Strength, Yield 90.0 MPa
13100 psi
ASTM-D638
Elongation at Break 3.0 %
3.0 %
ASTM-D638
Flexural Strength 115 MPa
16700 psi
ASTM-D790
Flexural Modulus 8.00 GPa
1160 ksi
ASTM-D790
Izod Impact, Notched 0.800 J/cm

@Temperature 23.0 °C
1.50 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 101 °C
214 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
DIN 53482
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
DIN 53482
Users viewing this material also viewed the following: