Material Notes:
Impact modified PBT for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Linear Mold Shrinkage 0.021 - 0.023 cm/cm
0.021 - 0.023 in/in
ISO 2577
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 250 °C
20 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO 527
Elongation at Break 70 %
70 %
ISO 527
Tensile Modulus 2.10 GPa
305 ksi
ISO 527
Flexural Strength 80.0 MPa
11600 psi
ISO 178
Flexural Modulus 2.20 GPa
319 ksi
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 180
8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60250
Users viewing this material also viewed the following: