Material Notes:
Description: Sphericel® 110P8 hollow glass spheres displace the same volume of resin as solid spheres of the same size, but are lighter. Using Sphericel® hollow glass spheres, plastics engineers can produce lighter-weight filled parts or use higher density resins without significant increases in part weight. Breakage of these tough hollow spheres is insignificant, they survive injection molding pressures of over 10,000 psi.Information provided by Potters Industries.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Particle Size 4.0 µm
4.0 µm
10% finer than
8.0 µm
8.0 µm
50% finer than
11.7 µm
11.7 µm
mean value
12 - 16 µm
12 - 16 µm
90% finer than
Descriptive Properties Value Comments
Color white
Composition Borosilicate Glass