Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering N60W Nitrile Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering N60W Nitrile Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
White Nitrile Butadiene Rubber (NBR), 55-65 °IRHD. Copolymer of acrylonitrile and butadiene. Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations Title 21 (CFR21), Section 177.2600.Applications: Material formulated for repeated use in equipment associated with the production of foodstuffs intended for human consumption.
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
°IRHD; ASTM D1415
67
67
°IRHD, +10 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 11.7 MPa
1700 psi
-10% change after 70 hours @ 100°C; ASTM D412
13.0 MPa
1890 psi
ASTM D412
Elongation at Break 262.5 %
262.5 %
-25% change after 70 hours @ 100°C; ASTM D412
350 %
350 %
ASTM D412
Compression Set 45 %
45 %
24 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F
Copyright © lookpolymers.com All Rights Reserved