Precision Polymer Engineering Z95Z Hydrogenated NBR Compound

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering Z95Z Hydrogenated NBR Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Peroxide cured and methacrylate modified, hydrogenated nitrile rubber, 80-92 °IRHD. Medium acrylonitrile content (ACN=36%). ASTM designation = HNBR.Applications: For uses where very high physical properties, abrasion resistance, low hysteresis and excellent flex-life are required. Where applicable, designed to withstand solutions between 3.5 to 13 pH and fluids similar to ASTM #1 oil and hot water, but also capable of maintaining physical properties at high temperatures.
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
°IRHD; ASTM D1415
91
91
°IRHD, +9 change after 70 hours @ 150°C; ASTM D1415
Tensile Strength, Yield 17.3 MPa
2510 psi
ASTM D412
19.895 MPa
2885.5 psi
15% change after 70 hours @ 150°C; ASTM D412
Elongation at Break 382.2 %
382.2 %
-9% change after 70 hours @ 150°C; ASTM D412
420 %
420 %
ASTM D412
Compression Set 40 %
40 %
24 hours @ 150°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 300 °C
>= 572 °F