Material Notes:
NT-C offers superior arc and heat resistance properties, with adequate strength properties to withstand mechanical stress and hold up in severe electrical insulating applications. NT-C does not promote combustion and will not ignite.Information provided by Pyrotek.
Physical Properties Metric English Comments
Specific Gravity 2.30 g/cc
2.30 g/cc
Water Absorption <= 0.50 %
<= 0.50 %
with silicone treatment
8.6 %
8.6 %
Mechanical Properties Metric English Comments
Flexural Strength 35.0 MPa
5080 psi
Compressive Strength 138 MPa
20000 psi
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
Thermal Properties Metric English Comments
Thermal Conductivity 0.140 W/m-K
0.972 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 550 °C
1020 °F
Continuous use
750 °C
1380 °F
Flammability, UL94 V-0
V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 6.00 kV/mm
152 kV/in
Arc Resistance >= 420 sec
>= 420 sec