Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
Pyrotek NT-C Electrical Insulating Material NT-C offers superior arc and heat resistance properties, with adequate strength properties to withstand mechanical stress and hold up in severe electrical insulating applications. NT-C does not pro.. |
|||
Specific Gravity | 2.30 - 2.70 g/cc | 2.30 - 2.70 g/cc | |
Parker Chomerics CHO-BOND 584-29 Conductive Adhesive Two-component, highly conductive adhesive system that combines the good adhesive characteristics of epoxy with the superior conductivity of silver. In addition to being available in bulk form, the m.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | ASTM D792 |
Quadrant EPP Fluorosint® 207 PTFE, Compression Molded Synthetic Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | ASTM D792 |
Parker Chomerics THERM-A-FORM 1642 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
Resin Technology Group KONA 870FT-FR Fire Retardant Epoxy Casting System Mix ratio 100 to 4 by weight.KONA 870 FTFR with HARDENER #9 is a versatile epoxy casting system that exhibits unusually high thermal conductivity and low thermal expansion. It is recommended for ele.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® GR-Fk Gap Filler Pad Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® GR-HFk Gap Filler Pad Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak.. |
|||
Specific Gravity | 2.30 - 2.40 g/cc @Temperature 25.0 °C |
2.30 - 2.40 g/cc @Temperature 77.0 °F |
|
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | Mixed |
Tra-Con Tra-Bond 2158 Heat Conductive Electrically Insulating Compound TRA-BOND 2158 is a flexible, thermal conductive epoxy system. It is used for staking transistors, diodes, resistors, integrated circuits and other heat-sensitive components to printed circuit boards.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
World Minerals Celite® Super Floss® MX Diatomaceous Earth Antiblock Additive Used as an antiblocking additive for polyethylene films. Exhibits minimal interactions with other additives in most LDPE and LLDPE resin systems.Antiblocking is accomplished via the varied particle.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
Aremco AREMCOLOX™ 502-1100 (Full-Fired) Dense Alumino-Silicate Good mechanical strength, and electrical and thermal resistance. For producing insulators, standoffs, feed-thrus, furnace carriers and brazing fixtures. Fabricate and fire yourself using conventio.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
Aremco Pyro-Paint™ 634-SIC High Temperature Refractory Coating This advanced silicon carbide, water-based coating reduces significantly the oxidation of graphite and carbon components and structures at temperatures to 2550 °F (1400 °C). Provides a hard surfac.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
World Minerals Celite® Micro-Ken® 801 Diatomaceous Earth Antiblock Additive Used as an antiblocking additive for polyethylene films. Exhibits minimal interactions with other additives in most LDPE and LLDPE resin systems.Antiblocking is accomplished via the varied particle.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
World Minerals Celite® Super Floss® Diatomaceous Earth Antiblock Additive Used as an antiblocking additive for polyethylene films. Exhibits minimal interactions with other additives in most LDPE and LLDPE resin systems.Antiblocking is accomplished via the varied particle.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
World Minerals Celite® Super Floss® E Diatomaceous Earth Antiblock Additive Used as an antiblocking additive for polyethylene films. Exhibits minimal interactions with other additives in most LDPE and LLDPE resin systems.Antiblocking is accomplished via the varied particle.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | mixed, uncured |
Atom Adhesives AA-SUPERTHERM 05 Epoxy Adhesive AA-SUPERTHERM 05 is a thixotropic (smooth paste) Pure Diamond ultra-high thermally conductive epoxy two-part adhesive that develops strong, durable, high-impact bonds at room temperature which impro.. |
|||
Specific Gravity | 2.30 - 3.00 g/cc | 2.30 - 3.00 g/cc | |
Reade Advanced Materials Montmorillonite - Smectite ((Na,Ca)(Al,Mg)6(Si4O10)3(OH)6-nH2O) Description: A clay mineral having a 2:1 expanding crystal lattice. Isomorphous substitution gives the various types and causes a net permanent charge balanced by cations in such a manner that water.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | ASTM D792 |
Quadrant EPP Semitron® ESd 500 HR PTFE, static dissipative, compression molded (ASTM Product Data Sheet) |