Pyrotek O1-C Fiber Seal Pre-cut Gasket

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek O1-C Fiber Seal Pre-cut Gasket.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silicone coated felt. Excellent resistance to vibration. Coating burns off at 315°C.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.256 g/cc
0.00925 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 650 °C
1200 °F
Continuous