Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 650 °C | 1200 °F | |
Pyrotek G-1 Low-Temperature Felt An inexpensive, tough material. Will not support combustion.Rolls:610 mm x 30.5 m 13 & 25 mm thickApplicationsHigh-temperature gasketsInformation provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | Continuous |
Pyrotek G-2 Fiber Seal Pre-cut Gasket A black, inexpensive material. Suitable for reusable gaskets.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | |
Pyrotek G-2 Low-Temperature Felt An inexpensive tough material.Dimensions610 mm x 30.5 m 25 mm thickApplicationsHigh-temperature gasketsInformation provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | Continuous |
Pyrotek IR-3 Fiber Seal Pre-cut Gasket A felt-like material which expands between 350°C and 540°C.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | |
Pyrotek IR-3 Low-Temperature Felt Felt-like material which expands between 350°C and 540°C.Custom Rolls:3 & 6 mm thickApplicationsCompressible gasketing Collector bar seals Siphon gaskets Flange gaskets Information provided by Pyr.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | for Continuous use with standard cloth exterior |
Pyrotek MT-29P Microporous Panel Insulation MT-29P is a unique panel insulation which offers exceptionally low thermal conductivity. The exterior of the panel is a glass fabric which maximizes the strength of the rigid interior panel.Applica.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | Continuous |
Pyrotek O1-C Fiber Seal Pre-cut Gasket Silicone coated felt. Excellent resistance to vibration. Coating burns off at 315°C.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | |
Pyrotek O-1C Low-Temperature Felt O-1 with a red silicone coating.Dimensions1524 mm x 22.9 m 6, 13, 25 mm thickApplicationsSiphon, air collection system, and carbon bake seals Makes an excellent air-tight, abrasion resistant seal In.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | Continuous |
Pyrotek T-1 Fiber Seal Pre-cut Gasket A dark brown, very strong and tough material.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | for Continuous use with standard cloth exterior |
Pyrotek MT-29L Microporous Ladle Lining Insulation MT-29L is a microporous insulation material covered with a flexible glass fabric. Parallel-stitched for ease of handling during installation, it is designed for use between ladle shells and the bac.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | for long term exposure |
Microtherm Group MT Thermosphere® Moldable Insulation Paste MT Thermosphere® is a low density temperature resistant paste with excellent thermal insulation properties from cryogenic to high temperature exposure. It is a perfectly seamless insulation syste.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | |
MetalTek MTEK 29-4 Cast UNS J92605 Heat Resistant Stainless Steel Restrict to low stress applications. Resists oxidation and high sulfur flue gas.Applications: Tuyeres, gas dampers, salt pots, support skids.Information provided by MetalTek |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | resistance to low cycle and thermal fatigue |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 10% Cold Work Tensile strength (ultimate and yield), elongation, and reduction of area values are for annealed then cold worked samples. This produces ASTM grain size 9.0. Other property values are typical of t.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | resistance to low cycle and thermal fatigue |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 15% Cold Work Tensile strength (ultimate and yield), elongation, and reduction of area values are for annealed then cold worked samples. This produces ASTM grain size 9.0. Other property values are typical of t.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | resistance to low cycle and thermal fatigue |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 20% Cold Work Tensile strength (ultimate and yield), elongation, and reduction of area values are for annealed then cold worked samples. This produces ASTM grain size 9.0. Other property values are typical of t.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | resistance to low cycle and thermal fatigue |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 30% Cold Work Tensile strength (ultimate and yield), elongation, and reduction of area values are for annealed then cold worked samples. This produces ASTM grain size 10.0. Other property values are typical of .. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | resistance to low cycle and thermal fatigue |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 40% Cold Work Tensile strength (ultimate and yield), elongation, and reduction of area values are for annealed then cold worked samples. This produces ASTM grain size 10.0. Other property values are typical of .. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | resistance to low cycle and thermal fatigue |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 5% Cold Work Tensile strength (ultimate and yield), elongation, and reduction of area values are for annealed then cold worked samples. This produces ASTM grain size 9.0. Other property values are typical of t.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | resistance to low cycle and thermal fatigue |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 1950°F (1070°C) Tensile strength (ultimate and yield), elongation, and hardness values are for samples annealed 1950°F (1070°C)/5 minutes/AC. This produces ASTM grain size 9.5. Other property values are ty.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | resistance to low cycle and thermal fatigue |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 1950°F (1070°C) + Aged 1400°F (760°C) Tensile strength (ultimate and yield), elongation, and hardness values are for samples annealed 1950°F (1070°C)/5 minutes/AC + Aged 1400°F (760°C)/100h/AC. This produces ASTM grain siz.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | resistance to low cycle and thermal fatigue |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 2150°F (1180°C) Tensile strength (ultimate and yield), elongation, and hardness values are for samples annealed 2150°F (1180°C)/5 minutes/AC. This produces ASTM grain size 5.5. Other property values are ty.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | resistance to low cycle and thermal fatigue |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 2150°F (1180°C) + Aged 1200°F (650°C) Tensile strength (ultimate and yield), elongation, and hardness values are for samples annealed 2150°F (1180°C)/5 minutes/AC + Aged 1200°F (650°C)/100h/AC. This produces ASTM grain siz.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | resistance to low cycle and thermal fatigue |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 2150°F (1180°C) + Aged 1400°F (760°C) Tensile strength (ultimate and yield), elongation, and hardness values are for samples annealed 2150°F (1180°C)/5 minutes/AC + Aged 1400°F (760°C)/100h/AC. This produces ASTM grain siz.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | Normal atmosphere |
Sinotek Materials Tungsten Disulfide (WS2) Powder, High-Purity Tungsten Disulfide powder mainly has applications in spraying, coating, carbon material, all sorts of grease, lubricating oil, friction materials and catalysts. Tungsten Disulfide has good resistan.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | |
Zircar Refractory Composites ZIRCAL-45 Refractory Board Type ZIRCAL-45 Refractory Board is a self supporting, high strength, rigid refractory product fabricated from calcium silicate, inert fillers and reinforcing agents. Its high structural strength com.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | |
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | in normal atmosphere |
BryCoat WS2 Tungsten Disulfide Coating WS2's unique, extensively modified lamellar composition of tungsten disulfide results in a high performance dry coating lubricant. A pressurized air application processes impinges a dry metallic co.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | Continuous |
Pyrotek G-1 Fiber Seal Pre-cut Gasket A black, inexpensive material. Will not support combustion.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | |
Pyrotek O-1 Low-Temperature Felt Excellent resistance to vibration. Not effected by 1.55 MPa steam.Dimensions1524 mm x 22.9 m 6, 13, 25 mm thickApplicationsHigh-density gaskets at elevated temperatures Initial systems, high pressu.. |
|||
Maximum Service Temperature, Air | 650 °C | 1200 °F | resistance to low cycle and thermal fatigue |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 1950°F (1070°C) + Aged 1200°F (650°C) Tensile strength (ultimate and yield), elongation, and hardness values are for samples annealed 1950°F (1070°C)/5 minutes/AC + Aged 1200°F (650°C)/100h/AC. This produces ASTM grain size 9.5. .. |