Qualchem Danamid AFCF-30 Polyamide 66, 30% Carbon Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Qualchem Zrt.
Trade Name Danamid
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Qualchem Danamid AFCF-30 Polyamide 66, 30% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reinforced with carbon fiber, antistatic and conductive.Information provided by Qualchem Zrt.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
DIN 53479
Filler Content 28 - 32 %
28 - 32 %
Linear Mold Shrinkage 0.010 - 0.015 cm/cm
0.010 - 0.015 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 200 MPa
>= 29000 psi
50 mm/min; ISO 527-1,2
Elongation at Break 3.0 %
3.0 %
ISO 527-1,2
Tensile Modulus >= 20.0 GPa
>= 2900 ksi
ISO 527-1,2
Flexural Strength >= 250 MPa
>= 36300 psi
10 mm/min; DIN 53452
Flexural Modulus >= 10.0 GPa
>= 1450 ksi
DIN 53452
Charpy Impact Unnotched >= 3.50 J/cm²

@Temperature 23.0 °C
>= 16.7 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
DIN 53461
Flammability, UL94 HB

@Thickness 4.00 mm
HB

@Thickness 0.157 in
MSZ 10383
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
DIN 53482
Processing Properties Metric English Comments
Moisture Content 1.3 - 2.0 %
1.3 - 2.0 %
DIN 53714