Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 129 - 166 °C | 265 - 330 °F | Mold Temperature |
Quantum Composites LYTEX® 4181 55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4181 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance.. |
|||
Processing Temperature | 129 - 166 °C | 265 - 330 °F | Mold Temperature |
Quantum Composites LYTEX® 4197 55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4197 is an epoxy high performance, 3K tow carbon fiber (PAN) reinforced engineered structural composite (ESC) molding compound designed for military and aerospace structural applications requi.. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Thermoforming Temp |
Alcoa KAMA 3000 High Impact Polystyrene (HIPS)
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an.. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Thermoforming Temp |
Alcoa KAMA 3210 Hi-Gloss Coextruded High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat.. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Thermoforming Temp |
Alcoa KAMA 3400 Super High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an.. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Thermoforming Temp |
Alcoa KAMA AgriHIPS 3500 AgriHIPS
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat.. |
|||
Processing Temperature | 120 - 166 °C | 248 - 331 °F | Mold temperature |
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC Lytex 4149 is a high-performance, 3K tow carbon fiber (PAN) reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical propert.. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Average value: 143 °C Grade Count:7 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | Molding |
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A30 General Purpose Molding Compound BMC A30 is a general purpose molding compound with good dimensional stability. Due to the excellent flow and controlled reactivity, BMC A30 is well suited for injection, transfer or compression mol.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A30-3021 General Purpose Molding Compound BMC A30-3021 is a low shrink, general purpose molding compound formulated for the lighting industry. A30-3021 is temperature stabilized for use in elevated temp. lighting applications. Due to the .. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A50-EG Low Glass, Encapsulation Grade Molding Compound BMC A50-EG is a low glass, encapsulation grade material. It is well suited for injection, transfer or compression molding of intricate parts. Typical applications are motor armatures and coils.Inf.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T14 General Purpose Molding Compound BMC T14 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T14 is well suited for injection, transfer or compression molding of intricate parts. Typica.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T15(GP) General Purpose Molding Compound BMC T15(GP) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GP) is well suited for a variety of applications. It is av.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical propertie.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS-15869 is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical pro.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T60 Grey Wear Resistant Molding Compound BMC T60 Grey is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T60-6002A-WG Wear Resistant Molding Compound BMC T60-6002A-WG is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost pe.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T60-6002-WG(15) Wear Resistant Molding Compound BMC T60-6002-WG-(15) is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cos.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T9 General Purpose Molding Compound BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A20-(a) High Strength Grade Molding Compound BMC A20 is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A20 is well suited for injection, transfer or compression molding o.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A50-MS General Purpose Molding Compound BMC A50-MS is a medium strength, high appearance, general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A50-MS is well suited for injection, transfer or compres.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T10(14) General Purpose Molding Compound BMC T10(14) is a general purpose, low shrink molding compound. Due to the excellent flow and controlled reactivity, BMC T10(14) is well suited for injection, transfer or compression molding of intr.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T15(GPS) General Purpose Molding Compound BMC T15(GPS) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPS) is well suited for injection, transfer or compression.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T15(GPT) General Purpose Molding Compound BMC T15(GPT) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPT) is well suited for injection, transfer or compression.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi.. |
|||
Processing Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC T60-6006 Wear Resistant Molding Compound BMC T60-6006 is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu.. |