Material Notes:
Available in North America Additive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Lubricated, Heat Stabilized, Impact Modifier and High FlowRoHS CompliantAuto Specifications: GM GMW16447P-PA66-T2 Color: BlackForm: Pellets Processing Method: Injection Molding Information provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Water Absorption 1.2 %
1.2 %
ASTM D570
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm

@Thickness 3.17 mm
0.016 - 0.020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Flexural Strength 74.5 MPa
10800 psi
ASTM D790
Flexural Modulus 2.24 GPa
325 ksi
ASTM D790
Izod Impact, Notched 1.76 J/cm
3.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 213 °C
415 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.2 °C
153 °F
Unannealed; ASTM D648