Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylon® N1240MGHL BK Nylon 6/6

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N1240MGHL BK Nylon 6/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Filler: Glass Fiber Reinforcement -15% Filler by Weight, Mineral -25% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated, Low Warpage and Heat StabilizedRoHS Compliant Auto Specifications: GM GMP.PA66.036R Color: BlackForm: Pellets Color: BlackInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183
Water Absorption 0.80 %

@Time 86400 sec
0.80 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955 and ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Rockwell M 98
98
ASTM D785
Tensile Strength at Break 113 MPa
16400 psi
ISO 527-2
114 MPa
16500 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D638
Flexural Strength 172 MPa
24900 psi
ISO 178
172 MPa
25000 psi
ASTM D790
Flexural Modulus 8.41 GPa
1220 ksi
ISO 178
8.62 GPa
1250 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 4.20 kJ/m²
2.00 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 229 °C
445 °F
Unannealed; ASTM D648