Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylon® N2040MGHL Nylon 6 (DAM)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N2040MGHL Nylon 6 (DAM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Water Absorption 0.90 %
0.90 %
24 hrs; ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
0.125 in; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Yield 131 MPa
19000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 190 MPa
27500 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
ASTM D257
Dielectric Strength 21.7 kV/mm
550 kV/in
ASTM D149
Processing Properties Metric English Comments
Melt Temperature 260 - 282 °C
500 - 540 °F
Mold Temperature 71.1 - 98.9 °C
160 - 210 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content 0.18 %
0.18 %
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Screw Speed 50 - 120 rpm
50 - 120 rpm
Descriptive Properties Value Comments
Holding Pressure 750 to 1400 psi
Injection Rate Fast
Users viewing this material also viewed the following: