Material Notes:
Relene L60075 is UV stabilized. It is available with a recommended service life of more then 5 years L60075 is suitable for applications where articles are exposed to sunlight e.g. soft drink crates, defense applications, and helmets.Information provided by Reliance Industries
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D1505
Melt Flow 8.2 g/10 min

@Load 2.16 kg
8.2 g/10 min

@Load 4.76 lb
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D638
Flexural Yield Strength 30.0 MPa
4350 psi
ASTM D790
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
Izod Impact, Notched 0.880 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 220 - 250 °C
428 - 482 °F
Recommended injection moulding temperature
Users viewing this material also viewed the following: