Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 30.0 MPa @Temperature 90.0 °C |
4350 psi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Flexural Yield Strength | 30.0 MPa @Temperature 90.0 °C |
4350 psi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilamid B3N Unfilled, Nucleated PA6 Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro.. |
|||
Flexural Yield Strength | 30.0 MPa | 4350 psi | ASTM D790 |
Reliance Industries Relene M60075 Polyethylene Relene M60075 is a High Density Polyethylene grade suitable for injection molding applications where good mechanical properties, gloss, dimensional stability, and good ESCR are required. This grade.. |
|||
Flexural Yield Strength | 30.0 MPa | 4350 psi | ASTM D790 |
North Wood Plastics HDPE with 60% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Flexural Yield Strength | 30.0 MPa | 4350 psi | ASTM D790 |
Reliance Industries Relene L60075 Polyethylene Relene L60075 is UV stabilized. It is available with a recommended service life of more then 5 years L60075 is suitable for applications where articles are exposed to sunlight e.g. soft drink crates.. |
|||
Flexural Yield Strength | 30.0 - 180 MPa | 4350 - 26100 psi | Average value: 86.8 MPa Grade Count:14 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Flexural Yield Strength | 30.0 - 30.0 MPa @Temperature 90.0 - 90.0 °C |
4350 - 4350 psi @Temperature 194 - 194 °F |
Average value: 30.0 MPa Grade Count:1 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Flexural Yield Strength | 30.0 - 145 MPa | 4350 - 21000 psi | Average value: 81.9 MPa Grade Count:10 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Flexural Yield Strength | 30.0 MPa | 4350 psi | ASTM Data |
BASF Capron® 8203C Nylon 6 (Conditioned)
(discontinued **) Capron 8203C is a high viscosity, nylon 6 extrusion compound, possessing a modified crystalline structure for increased property performance and faster set up for tubing and cable applications. It.. |
|||
Flexural Yield Strength | 30.0 - 30.0 MPa @Temperature 90.0 - 90.0 °C |
4350 - 4350 psi @Temperature 194 - 194 °F |
Average value: 30.0 MPa Grade Count:1 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Flexural Yield Strength | 30.0 MPa | 4350 psi | ASTM Data |
BASF Capron® 8253 Impact Modified Nylon 6 (Conditioned)
(discontinued **) Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions.. |
|||
Flexural Yield Strength | 30.0 MPa | 4350 psi | ASTM Data |
BASF Capron® 8351 Impact Modified Nylon 6 (Conditioned)
(discontinued **) Capron 8351 is a type 6 polyamide graft copolymer developed for injection molding applications requiring a high level of toughness combined with moderate flexibility and faster cycles. It is also .. |
|||
Flexural Yield Strength | 30.0 MPa | 4350 psi | ASTM D790 |
Tipco Tipcolene® IA 933 IN - 20% Talc/Mineral Reinforced Polypropylene Copolymer, High Flow, Stiffness & Impact Strength 20% Mineral Reinforced, High Stiffness, High Impact PP CopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,