Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Reliance Industries Repol H200MA Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Repol H200MA Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
REPOL Polypropylene H200MA is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H200MA is recommended for use in injection molding processes. It is an ideal material for molding articles with intricate, long flow paths and multicavity molding. Repol H200MA contains antistatic agent that reduces static charge build up on products.Features:Low static charge build-up and reduced dust pickupGood flow behavior Consistent processabilityExcellent color stabilityInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
50mm/min; ASTM D638
Elongation at Yield 11 %
11 %
50mm/min; ASTM D638
Flexural Modulus 1.65 GPa
239 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.270 J/cm

@Temperature 23.0 °C
0.506 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648
Users viewing this material also viewed the following: