Material Notes:
REPOL Polypropylene T100MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol T100MK is recommended for use in injection molding & stretch blow molding processes. It is an ideal material for attaining high clarity in housewares, syringes and ISBM products. Repol T100MK contains clarifier and antistatic agent that reduces static charge buildup on products. Features: Consistent processabilityGood clarity Good impact strengthSuperior mechanical propertiesLow static charge build-up and reduced dust pickupInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
50mm/min; ASTM D638
Elongation at Yield 12 %
12 %
50mm/min; ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 145 °C
293 °F
DSC second heating; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648