Material Notes:
Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Viscosity 310000 cP
310000 cP
Melt Viscosity, 200°C, 1000 sec-1; ASTM D3825
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 6.8 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.8 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
9.0 g/10 min

@Load 5.00 kg,
Temperature 220 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 428 °F
ISO 1133
Melt Index of Compound 37 g/10 min

@Load 10.0 kg,
Temperature 220 °C
37 g/10 min

@Load 22.0 lb,
Temperature 428 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 42.0 MPa
6090 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 11 %
11 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 2.1 %
2.1 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 2.41 GPa
350 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 73.0 MPa
10600 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.72 GPa
395 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Dart Drop, Total Energy 41.0 J

@Temperature 23.0 °C
30.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 79.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 79.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C

@Thickness 3.20 mm
181 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C

@Thickness 3.20 mm
162 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 90.0 °C
194 °F
Rate B/50; ASTM D1525
UL RTI, Electrical 60.0 °C
140 °F
UL 746B
UL RTI, Mechanical with Impact 60.0 °C
140 °F
UL 746B
UL RTI, Mechanical without Impact 60.0 °C
140 °F
UL 746B
Flammability, UL94 V-0

@Thickness 2.31 mm
V-0

@Thickness 0.0909 in
UL 94
5VB

@Thickness 2.48 mm
5VB

@Thickness 0.0976 in
UL 94