Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C @Thickness 3.20 mm |
181 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® FR23 ABS Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C @Thickness 3.20 mm |
181 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® FR23 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Network Polymers MS 150 IF Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Network Polymers NPP 20-2501 C/AS Description: Random Copolymer Polypropylene, Clarified, with AntistatInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYabs V0E ABS, Flame Retardant Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ISO 75/Method Bf |
Premix Thermoplastics PRE-ELEC® PS 1328 PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
SABIC PP681K Polypropylene Random Copolymer for Injection Molding Product Description: PP 681K is specially developed for producing injection molded articles with high clarity and also has better impact properties than homo PP counterparts.PP 681K has the followi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 - 210 °C | 181 - 410 °F | Average value: 160 °C Grade Count:22 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | |
LyondellBasell Lupolen® 5621 D HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Flint Hills P5L2Z-038 Random Copolymer Polypropylene Random copolymer, USP Class VI certified, and FDA compliant.Features: Hydrotalcite.Applications: Injection molding: extrusion blow molding and hot fill applications.Former Huntsman polypropylene pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ISO 75 |
LyondellBasell Hifaxâ„¢ CB228 Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good paintability, good processabilityApplications: aut.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ISO 75-1/-2 |
Styrolution Polystyrol 486 M GR 2 PS Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ISO 75 |
Styrolution PS 486N HIPS Styrolution PS 486N is a normal flowing, high impact grade that is especially suitable for blends with a high proportion of general purpose polystyrene (preferably Styrolution PS 165N of Styrolution.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Borealis Bormed™ RB845MO Random Copolymer for Healthcare Applications Bormed RB845MO is a random copolymer for blow molding with very good transparency and high contact clarity, very good gloss and surface finish. Bottles in sizes up to 2 quarts molded from Bormed RB.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Total PPR 6523WZ Polypropylene, Nucleated Random Copolymer for Injection Molding Impact - 6523WZ produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.Antistat - 6523WZ contains an antistat to help protect molded parts from dust acc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite 105E3V36327 Acetate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite 360E461312 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite 572E3720012 Cellulose Acetate Butyrate, Clear, Trsp Applications:FilmsProfilesSheetProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a wa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite Propionate 377E4861312 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite Propionate 383A2R30012 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM-D648 |
Braskem PRB 0131 RACO Random Polypropylene Copolymer PRB 0131 is a low melt flow rate random copolymer with high transparency. This resin is designed for thermoforming, blow molding, and extrusion. This product exhibits excellent processability, low h.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Braskem RP 141 Injection Molding Polypropylene Description: RP 141 is a high melt flow rate random copolymer designed for injection molding. This product offers outstanding transparency, very good stiffness/impact strength balance and excellent .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | |
BASF Polystyrol® 475 K Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade with particularly good creep strength.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | |
BASF Polystyrol® 486 M Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H). Suitable for dairy packaging.Data was co.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Braskem CP 144 Coating Polypropylene Information provided by Braskem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612
(Unverified Data**) Zytel® LC6210 BK010 is a highly toughened, heat stabilized polyamide 612 for extrusion, blow molding or processing by other techniques requiring high melt viscosity. It was previously coded Zytel®.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite Butyrate 465A3720010 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 10%. Weight loss on heating = 0.9% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
LyondellBasell Astryn 73A6-3 Polypropylene Copolymer, 30% Calcium Carbonate Key Features: medium high melt flow, medium modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, excellent chemical resistance, excellent aesthetics, high gloss, .. |