Material Notes:
LNP* COLORCOMP* DX99340H is an unfilled Polycarbonate resin. Added feature of this grade is: Healthcare.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Melt Flow 23.8 g/10 min

@Load 1.20 kg,
Temperature 300 °C
23.8 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Melt Index of Compound 23 g/10 min

@Load 1.20 kg,
Temperature 300 °C
23 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Izod Impact, Notched 6.94 J/cm
13.0 ft-lb/in
ASTM D256