Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP FARADEX KX88084 POM (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP FARADEX KX88084 POM (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Faradex* KX88084 is a compound based on POM resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 56.0 MPa
8120 psi
5 mm/min; ISO 527
Elongation at Break 11 %
11 %
5 mm/min; ISO 527
Flexural Strength 62.0 MPa
8990 psi
2 mm/min; ISO 178
Flexural Modulus 2.30 GPa
334 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257