Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Faradex DS0026 PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Faradex DS0026 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Faradex* DS0026 is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel Fiber. Added features include: EMI/RFI Shielding, Flame Retardant, Non-Brominated & Non-Chlorinated Flame Retardant,Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
Water Absorption 0.21 %

@Temperature 23.0 °C,
Time 86400 sec
0.21 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 53.0 MPa
7690 psi
5 mm/min; ISO 527
Tensile Strength, Yield 58.0 MPa
8410 psi
5 mm/min; ISO 527
Elongation at Yield 3.4 %
3.4 %
5 mm/min; ISO 527
Tensile Modulus 2.90 GPa
421 ksi
1 mm/min; ISO 527
Flexural Yield Strength 93.0 MPa
13500 psi
2 mm/min; ISO 178
Flexural Modulus 2.80 GPa
406 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
35.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 122 °C
252 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 112 °C
234 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D 257
Shielding Effectiveness 30 - 45 dB

@Thickness 3.00 mm
30 - 45 dB

@Thickness 0.118 in
SABIC Method