Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP DCL32 PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DCL32 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* DCL32 is a compound based on Polycarbonate resin contqaining Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Water Absorption 0.18 %

@Time 86400 sec
0.18 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 107 MPa
15500 psi
5 mm/min; ISO 527
Elongation at Break 1.9 %
1.9 %
5 mm/min; ISO 527
Tensile Modulus 8.00 GPa
1160 ksi
1 mm/min; ISO 527
Flexural Yield Strength 151 MPa
21900 psi
2 mm/min; ISO 178
Flexural Modulus 6.90 GPa
1000 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
11.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 82.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
45.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 142 °C
288 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257