Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP PFP36 PA 6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP PFP36 PA 6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* PFP36 is a compound based on Nylon 6 containing Glass Fiber and PTFE/Silicone. Characteristics are Impact Modifier.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.012 - 0.014 cm/cm

@Time 86400 sec
0.012 - 0.014 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
ISO 527
Elongation at Break 6.0 - 8.0 %
6.0 - 8.0 %
ISO 527
Tensile Modulus 3.20 GPa
464 ksi
1 mm/min; ISO 527
Flexural Strength 80.0 MPa
11600 psi
ISO 178
Flexural Modulus 3.10 GPa
450 ksi
ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C
136 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Users viewing this material also viewed the following: