Material Notes:
LNP* LUBRICOMP* DX99854 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D 792
Moisture Absorption at Equilibrium 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
50% RH; ASTM D 570
Mechanical Properties Metric English Comments
Tensile Strength at Break 63.0 MPa
9140 psi
ASTM D 638
Elongation at Break 50 - 75 %
50 - 75 %
ASTM D 638
Flexural Strength 96.0 MPa
13900 psi
ASTM D 790
Flexural Modulus 2.46 GPa
357 ksi
ASTM D 790
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Coefficient of Friction, Dynamic 0.21
0.21
ASTM D 3702 Modified
Coefficient of Friction, Static 0.21
0.21
ASTM D 3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 128 °C

@Thickness 3.20 mm
262 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Users viewing this material also viewed the following: