Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON CD000 PS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON CD000 PS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-kon* CD000 is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 26.0 MPa
3770 psi
5 mm/min; ISO 527
Elongation at Break >= 10 %
>= 10 %
5 mm/min; ISO 527
Flexural Strength 37.0 MPa
5370 psi
2 mm/min; ISO 178
Flexural Modulus 1.40 GPa
203 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1A
Electrical Properties Metric English Comments
Surface Resistance 1000 ohm - 1e+05
1000 ohm - 1e+05
ASTM D257