SABIC Innovative Plastics LNP STAT-KON SC004 PA 12 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON SC004 PA 12 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-kon* SE004 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
5 mm/min; ISO 527
Elongation at Break 2.0 - 4.0 %
2.0 - 4.0 %
5 mm/min; ISO 527
Tensile Modulus 10.3 GPa
1490 ksi
1 mm/min; ISO 527
Flexural Strength 171 MPa
24800 psi
2 mm/min; ISO 178
Flexural Modulus 7.90 GPa
1150 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
Electrical Properties Metric English Comments
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257