SABIC Innovative Plastics LNP Stat-kon CX01039 PS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Stat-kon CX01039 PS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-kon* CX01039 is a compound based on Polystyrene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.0 MPa
5950 psi
5 mm/min; ISO 527
Elongation at Break 1.3 %
1.3 %
5 mm/min; ISO 527
Flexural Strength 71.0 MPa
10300 psi
2 mm/min; ISO 178
Flexural Modulus 4.90 GPa
711 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Electrical Properties Metric English Comments
Surface Resistance 1000 - 1.00e+6 ohm
1000 - 1.00e+6 ohm
ASTM D 257