Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | ISO 180 |
Premix Premi-Glas® 1266 (Injection Compression Molded) Glass Reinforced TMC Description: Premi-Glas® 1266 is a glass reinforced thermoset molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injection/Co.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | ISO 180 |
Premix Premi-Glas® 1268 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1268 is a fiberglass reinforced thermoset thick molding compound for composite power train applications such as valve covers and timing gear covers.Key features and benefits are:Ideal f.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Faradex AS0029 ABS (Europe-Africa-Middle East) LNP* Faradex* AS-1002 FR is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: Flame Retardant, EM.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Konduit MT00EL PP LNP* Konduit* MT00EL is a Polypropylene base resin with thermal fillers. Characteristics of this grade are Thermal Conductivity and it is Low Extraactible.This data was supplied by SABIC-IP for th.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP AFP26 ABS (Europe-Africa-Middle East) LNP* Lubricomp* AFP26 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, PTFE, Silicone. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP BX05030 SAN (Europe-Africa-Middle East) LNP* Lubricomp* BX05030 is a compound based on Styrene Acrylonitrile resin containing Mineral, Graphite. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP CGI11 PS (Europe-Africa-Middle East) LNP * Lubricomp* CGI11 is a compound based on Polystyrene resin containing Graphite. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 10.0 - 33.0 kJ/m² | 4.76 - 15.7 ft-lb/in² | Average value: 17.2 kJ/m² Grade Count:6 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 - 90.0 kJ/m² @Temperature -30.0 - -30.0 °C |
4.76 - 42.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 63.5 kJ/m² Grade Count:6 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | ASTM D256 |
Mitsui APELâ„¢ APL5014DP Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | ASTM D256 |
Mitsui APELâ„¢ APL6015T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 180/1U |
SYNTHOS Krasten® 152 General Purpose Polystyrene Improved heat resistance, very good rheological properties.Examples of Application:Injection moulding – vegetable boxes for refrigerators, shower enclosure panels, CD and DVD cases. Blends with.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP LNP LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing 20% Glass Fiber and 15% PTFE. Added features of this material include: Heat Stabilized, Low Extractable, Wear Resistant... |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp RL0049 PA 66 LNP* Lubricomp* RL0049 is a compound based on Nylon 66 resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant.This data was supplied.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RL0049S PA 66 LNP LUBRICOMP* RL0049S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Flame Retardant, Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon CX01039 PS (Europe-Africa-Middle East) LNP* Stat-kon* CX01039 is a compound based on Polystyrene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | |
Shandong Rike Chemical RIKEâ„¢ RK-521 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp CF004 PS (Europe-Africa-Middle East) LNP* Thermocomp* CF004 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp CF006 PS (Europe-Africa-Middle East) LNP* Thermocomp* CF006 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP KB008 Acetal Copolymer LNP THERMOCOMP* KB008 is a compound based on Acetal Copolymer resin containing 40% Glass Bead. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WH0270F PBT LNP* Thermocomp* WH0270F is a dense compound based on PBT. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Europe-Africa-Middle East) LNP* STAT-KON* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containg Carbon Fiber. Added features include: Electrically Conductive |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp WH0270FX_WH5A289 PBT 2.7 specific gravity PBTThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | |
Goodfellow TPX® DX845 Extrusion Grade Polymethylpentene This grade is highly recommended for film extrusion; also for injection molding, fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensiv.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | Typical; ISO 180 |
Axion Polymers Axpoly® PS02 1010 Medium Impact Polystyrene PS02 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin co.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | ISO 180/1U |
A.D. Compound Adene NCQA Homopolymer 40% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Izod Impact, Unnotched (ISO) | 10.0 - 80.0 kJ/m² | 4.76 - 38.1 ft-lb/in² | Average value: 34.7 kJ/m² Grade Count:9 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 - 20.0 kJ/m² | 4.76 - 9.52 ft-lb/in² | Average value: 16.0 kJ/m² Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP CX94108 PS (Europe-Africa-Middle East) LNP* LUBRICOMP* CX94108 is a compound based on Polystyrene resin containing Proprietary Lubricant. Added features include: Internally Lubricated. |