Material Notes:
LNP STAT-KON* DX92440 is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D 955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm

@Time 86400 sec
0.0080 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 49.0 MPa
7110 psi
ASTM D 638
Tensile Strength, Yield 57.0 MPa
8270 psi
ASTM D 638
Elongation at Break 7.8 %
7.8 %
ASTM D 638
Elongation at Yield 4.3 %
4.3 %
ASTM D 638
Flexural Strength 99.0 MPa
14400 psi
ASTM D 790
Flexural Modulus 2.90 GPa
421 ksi
ASTM D 790
Izod Impact, Notched 0.650 J/cm

@Temperature 23.0 °C
1.22 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 13.08 J/cm

@Temperature 23.0 °C
24.50 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C

@Thickness 3.20 mm
124 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Flammability, UL94 V-0

@Thickness 1.65 mm
V-0

@Thickness 0.0650 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 10000 ohm - 1e+05
10000 ohm - 1e+05
ASTM D 257