Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP 67001XXH PBT+PC

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP 67001XXH PBT+PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* 67001XXH is a compound based on PC + PBT resin containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added features include: High antimicrobial performance, high impact, heat and chemical resistance. Improved retention of mechanical properties under UV exposure.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Moisture Absorption 0.100 %
0.100 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Time 86400 sec
0.0050 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm

@Time 86400 sec
0.0060 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 49.0 MPa
7110 psi
Type I, 5 mm/min; ASTM D638
50.0 MPa
7250 psi
5 mm/min; ISO 527
Tensile Strength, Yield 53.0 MPa
7690 psi
5 mm/min; ISO 527
54.0 MPa
7830 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 110 %
110 %
Type I, 5 mm/min; ASTM D638
120 %
120 %
5 mm/min; ISO 527
Elongation at Yield 4.6 %
4.6 %
Type I, 5 mm/min; ASTM D638
4.6 %
4.6 %
5 mm/min; ISO 527
Tensile Modulus 2.11 GPa
306 ksi
1 mm/min; ISO 527
2.20 GPa
319 ksi
5 mm/min; ASTM D638
Flexural Strength 78.0 MPa
11300 psi
ISO 178
Flexural Yield Strength 81.0 MPa
11700 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
2 mm/min; ISO 178
2.17 GPa
315 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1A
Dart Drop, Total Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
Impact Test 58.0 J
42.8 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 89.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
49.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
50.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
110 °C

@Thickness 3.20 mm
230 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
95.0 °C

@Thickness 3.20 mm
203 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: