Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP BF006 SAN (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , SAN Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP BF006 SAN (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* BF006 is a compound based on Styrene Acrylonitrile resin containing Glass Fiber.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Water Absorption 0.30 %

@Time 86400 sec
0.30 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0014 cm/cm
0.0014 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 91.0 MPa
13200 psi
5 mm/min; ISO 527
Elongation at Break 1.0 %
1.0 %
5 mm/min; ISO 527
Tensile Modulus 9.50 GPa
1380 ksi
1 mm/min; ISO 527
Flexural Yield Strength 109 MPa
15800 psi
2 mm/min; ISO 178
Flexural Modulus 7.80 GPa
1130 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 36.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
20.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 58.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
32.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
226 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
217 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94