Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP COLORCOMP J1000R PES (Europe-Africa-Middle East) LNP* COLORCOMP* J1000R is a compound based on Polyethersulfone resin. Added features include : Mold Release |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP 9X98026 PA 46 (Europe-Africa-Middle East) LNP* Lubricomp* 9X98026 is a compound based on PA4.6 resin containing Barium Sulfate, PTFE and Carbon Fiber |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 20.0 °C |
32.2 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® SMT-B-1™ Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA). It is formulated with a unique resin system that min.. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 20.0 °C |
32.2 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® SMT-B-1LV Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA). Using an improved optimized filler system, it provide.. |
|||
CTE, linear, Transverse to Flow | 58.0 - 75.0 µm/m-°C | 32.2 - 41.7 µin/in-°F | Average value: 66.1 µm/m-°C Grade Count:8 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C | 32.2 µin/in-°F | |
Idemitsu Kosan Xarec® WA 210 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified, Improved Mold Release. Used in Automotive and Industrial applications. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
32.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA6.10 LNP* LUBRICOMP* QCL34 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36AS is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp UFL36ASP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36ASP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE.
Added features include Internally Lubricated, Heat Stabilized.This data was supplied by SABIC-IP f.. |
|||
CTE, linear, Transverse to Flow | 57.9 µm/m-°C @Temperature -30.0 - 30.0 °C |
32.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC LNP* STAT-KON* DE002 is a Polycarbonate base resin containing 10% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
32.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC (Asia Pacific) LNP* Stat-Kon* DE002 is a Polycarbonate containing Carbon Fiber. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DE006 PC (Europe-Africa-Middle East) LNP* Stat-kon* DE006 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP BF006 SAN (Europe-Africa-Middle East) LNP* THERMOCOMP* BF006 is a compound based on Styrene Acrylonitrile resin containing Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UF007SXC PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF007SXC is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include : Heat Stabilized . |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 23.0 - 150 °C |
32.2 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem LTX931A PEI Blend (Europe-Africa-Middle East) Post-industrial recycle based, 30% glass fiber filled, high flow Polyetherimide blend. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
32.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP D452 PC COPOLYMER (Asia Pacific) LNP* Thermocomp* D452 (or EXTC8202) is a compound based on SABIC unique Polycarbonate copolymer resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, .. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C | 32.2 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSLR BK420 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin with improved hydrolysis resistance.. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C | 32.2 µin/in-°F | ISO 11359 |
BASF Ultramid® 8260 40% Mineral Filled PA6 (Dry) Ultramid 8260 is a 40% mineral reinforced PA6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low.. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C | 32.2 µin/in-°F | ISO 11359 |
BASF Ultramid® 8260 HS PA6 (Dry) |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 20.0 °C |
32.2 µin/in-°F @Temperature 68.0 °F |
ISO data |
BASF Capron® 8260 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 is a 40% mineral reinforced polyamide 6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability includi.. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU (Europe-Africa-Middle East) LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 58.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON RX00078 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX00078 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |