SABIC Innovative Plastics LNP THERMOCOMP MF00AS PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP MF00AS PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP THERMOCOMP* MF00AS is a compound based on Polypropylene resin containing 50% Glass Fiber. Added features of this material include: Chemically Coupled.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm

@Time 86400 sec
0.0080 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 87.0 MPa
12600 psi
ASTM D638
Elongation at Break 1.6 %
1.6 %
ASTM D638
Flexural Strength 149 MPa
21600 psi
ASTM D790
Flexural Modulus 11.03 GPa
1600 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm
5.99 ft-lb/in
ASTM D4812