Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP MX88028 PP (Asia Pacific)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP MX88028 PP (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* MX88028 is a compound based on Polypropylene resin containing Glass Fiber.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Time 86400 sec
0.0050 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 3.2 %
3.2 %
ASTM D638
Tensile Modulus 3.61 GPa
524 ksi
50 mm/min; ASTM D638
Flexural Strength 75.0 MPa
10900 psi
ASTM D790
Flexural Modulus 2.82 GPa
409 ksi
ASTM D790
Izod Impact, Notched 0.260 J/cm
0.487 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.94 J/cm
7.38 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C

@Thickness 3.20 mm
275 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: