SABIC Innovative Plastics LNP THERMOCOMP OF008G PPS - LINEAR

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP OF008G PPS - LINEAR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* OF008G is a compound based on PPS - Linear containing 15% Glass Fiber, 25% Milled Glass.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm

@Time 86400 sec
0.0020 - 0.0050 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 104 MPa
15100 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 1.9 %
1.9 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 8.84 GPa
1280 ksi
5 mm/min; ASTM D638
Flexural Strength 157 MPa
22800 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9.30 GPa
1350 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.680 J/cm
1.27 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.95 J/cm
7.40 ft-lb/in
ASTM D4812