Polymer Property : Flexural Modulus = 9.30 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 9.30 GPa
1350 ksi
ASTM D790
Nylene® PA6 Glass Filled 5233 HS Nylon 6
33% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Flexural Modulus 9.30 GPa

@Temperature 23.0 °C
1350 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB SCANBLEND P AP2060 F30 PBT/ASA, Glass Fiber Reinforced
Information provided by Polykemi AB
Flexural Modulus 9.30 - 22.0 GPa
1350 - 3190 ksi
Average value: 14.4 GPa Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
Flexural Modulus 9.30 GPa
1350 ksi
ISO 178
Solvay TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, DRY
Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL C 218 MZ20 V10 offe..
Flexural Modulus 9.30 GPa
1350 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RFL16 PA 66 (Asia Pacific)
LNP LUBRICOMP* RFL16 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 9.30 GPa
1350 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp RFL16S PA 66
LNP* Lubricomp* RFL16S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized.This data was supplied by ..
Flexural Modulus 9.30 GPa
1350 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp RFL16S PA 66 (Asia Pacific)
LNP* Lubricomp* RFL16S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized.This data was supplied by ..
Flexural Modulus 9.30 GPa
1350 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RFL26S PA 66
LNP* LUBRICOMP* RFL26S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized.
Flexural Modulus 9.30 GPa
1350 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 (Asia Pacific)
LNP* Lubricomp* RFL36L is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Flexural Modulus 9.30 GPa
1350 ksi
ISO 178
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS
LNP STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This dat..
Flexural Modulus 9.30 GPa
1350 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp RF0069 PA 66 (Europe-Africa-Middle East)
Flame retarded, 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 9.30 GPa
1350 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
Flexural Modulus 9.30 GPa
1350 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Asia Pacific)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
Flexural Modulus 9.30 GPa
1350 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Europe-Africa-Middle East)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
Flexural Modulus 9.30 GPa
1350 ksi
ISO 178
Wellman Wellamid® GF33-66 22LH-N 33% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Flexural Modulus 9.30 GPa
1350 ksi
ISO 178
Wellman Wellamid® GF33-66/6 XE-N 33% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
Flexural Modulus 9.30 GPa
1350 ksi
ISO 178-93
Wellman Wellamid® GF33-66/6 XE-NBK1 33% Glass Fiber Reinforced Nylon 66/6
Description: Glass Fiber Reinforced Nylon 66/6Information provided by Wellman.
Flexural Modulus 9.30 GPa
1350 ksi
ISO 178-93
Wellman Wellamid® MRGF25/15 42H-BKJA6A Nylon 6, 25% Mineral and 15% Glass Reinforced
Ford JA6A color matchedAll information provided by Wellman Engineered Resins.
Flexural Modulus 9.30 GPa
1350 ksi
ASTM D790
Toyobo Vylopet® EMC120S Glass Reinforced Polyester, Standard Grade
Key Feature: Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strengt..
Flexural Modulus 9.30 GPa
1350 ksi
ISO 178
DuPont Performance Polymers Rynite® 935 BK505 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced Polyethylene Terephthalate Rynite 935 BK505 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti..
Flexural Modulus 9.30 GPa
1350 ksi
DAM; ISO 178
DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66  (Unverified Data**)
33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L BK031 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont ..
Flexural Modulus 9.30 GPa
1350 ksi
DAM; ISO 178
DuPont Performance Polymers Zytel® 70G33L BK031 Nylon 66  (Unverified Data**)
33% Glass Reinforced Polyamide 66Zytel 70G33L BK031 is a 33% glass fiber reinforced black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Flexural Modulus 9.30 GPa
1350 ksi
DAM; ISO 178
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Flexural Modulus 9.30 GPa
1350 ksi
2 mm/min; ISO 178
Eurostar Starflam RF0069 PA66, 30% Glass Fiber, Flame Retardant, Injection Molded
Starflam RF0069 is a Flame Retardant, 30% Glass Reinforced Polyamide 66 Injection Molding Resin (also known as PA66 30V U2 Z79 or RF1006Z590)Information provided by Eurostar.
Flexural Modulus 9.30 GPa
1350 ksi
ISO 178
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, Conditioned
Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when..
Flexural Modulus 9.30 GPa
1350 ksi
ISO 178
BASF Ultramid® S3WG7 Balance 35% Glass Filled PA 610 (Dry)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Flexural Modulus 9.30 GPa
1350 ksi
ASTM D790
A. Schulman ComAlloy Hiloy® 753 Glass Reinforced, Flow Enhanced, PPS Alloy, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 9.30 GPa

@Temperature 23.0 °C
1350 ksi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® FGFE5171 NC010C Nylon 66  (Unverified Data**)
Zytel® FGFE5171 NC010C is a 33% glass filled nylon 66 resin. It has been developed for consideration into applications such as parts for the food industry.Information provided by DuPont Performance..
Flexural Modulus 9.30 GPa
1350 ksi
ISO 178
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM
Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters..
Flexural Modulus 9.30 GPa
1350 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp IF006S PA6.12
LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas ..