SABIC Innovative Plastics LNP THERMOCOMP RX05491 PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP RX05491 PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* RX05491 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 206 MPa
29900 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 310 MPa
45000 psi
ASTM D790
Flexural Modulus 14.54 GPa
2109 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 242 °C

@Thickness 3.20 mm
468 °F

@Thickness 0.126 in
unannealed; ASTM D648