SABIC Innovative Plastics LNP THERMOCOMP UX05504 PPA (Asia Pacific)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP UX05504 PPA (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* UX05504 is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 164 MPa
23800 psi
ISO 527
Tensile Strength, Yield 12.0 MPa
1740 psi
ISO 527
Elongation at Break 2.0 %
2.0 %
ISO 527
Flexural Strength 295 MPa
42800 psi
ISO 178
Flexural Modulus 10.0 GPa
1450 ksi
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 39.0 kJ/m²
18.6 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af