Material Notes:
LNP VERTON* PX00700 is a compound based on Nylon 6 resin containing proprietary fillers. Added feature of this grade is: Structural.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 188 MPa
27300 psi
ISO 527
Elongation at Break 2.7 %
2.7 %
ISO 527
Tensile Modulus 9.51 GPa
1380 ksi
1 mm/min; ISO 527
Flexural Strength 249 MPa
36100 psi
ISO 178
Flexural Modulus 8.21 GPa
1190 ksi
ISO 178
Izod Impact, Notched (ISO) 31.0 kJ/m²
14.8 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 73.0 kJ/m²
34.7 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 214 °C
417 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Users viewing this material also viewed the following: