SABIC Innovative Plastics NORYL EM7304F PPE+PS

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL EM7304F PPE+PS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
15% glass reinforced, high flow with enhanced polyurethane foam adhesion for instrument panel retainers.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0030 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm

@Thickness 3.20 mm
0.0025 - 0.0045 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 77.0 MPa
11200 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 2.0 %
2.0 %
Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 108 MPa
15700 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 4.55 GPa
660 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 123 °C

@Thickness 6.40 mm
253 °F

@Thickness 0.252 in
unannealed; ASTM D648